91做厙

Skip to main content
SHARE
Publication

The Effect of Water Vapor and Superalloy Composition on Thermal Barrier Coating Lifetime...

by Bruce A Pint, James A Haynes, Kinga A Unocic, Ying Zhang
Publication Type
Conference Paper
Publication Date
Page Numbers
723 to 732
Publisher Location
Warrendale, Pennsylvania, United States of America
Conference Name
Superalloys 2012
Conference Location
Seven Springs, Pennsylvania, United States of America
Conference Sponsor
TMS
Conference Date
-